Galvanic Corrosion Compatibility Checker

When two different metals touch in the presence of an electrolyte, the more active one corrodes faster. This checker compares their positions in the galvanic series and rates the risk for the environment, as a first screen before choosing fasteners, fittings or isolation kits.

Inputs

Results

Potential difference
0.53
Metal that corrodes (anode)
Carbon and low-alloy steel
Risk
High: isolate the metals or choose a compatible pair
  • Potentials are approximate values for flowing seawater. Real behaviour depends on area ratio, temperature, flow, oxygen and conductivity.
  • Never coat only the anode: a small coating defect concentrates attack on the anode.

RefENG-MAT-022
MethodPotential difference from the galvanic series in seawater; screening limits by environment
UnitsSI
Date2026-11-23

Working

Calculated in SI base units; inputs are converted from the units you choose.

  1. Corrosion potentials (V vs SCE, seawater)Carbon and low-alloy steel: -0.61 V; Stainless steel 304/316 (passive): -0.08 V
  2. Potential differenceΔE = |E₁ − E₂|ΔE = 0.53 V
  3. Screening limit for this environment0.25 V

Area ratio matters most

A small anode coupled to a large cathode corrodes very quickly; the reverse is usually tolerable. Carbon steel bolts in a stainless steel plate fail fast, while stainless bolts in a carbon steel plate are generally acceptable.

Screening limits

Common design guidance limits the potential difference to about 0.15 V for immersed or harsh conditions, 0.25 V for normal outdoor exposure and 0.5 V for dry, controlled interiors.

Assumptions and limits

  • Seawater galvanic series at about 25 °C.
  • Metals in electrical contact and wetted by an electrolyte.

References

  • ASTM G82, Development and use of a galvanic series for predicting galvanic corrosion performance.
  • MIL-STD-889, Dissimilar metals.

Questions

Can I use stainless steel bolts in aluminium?
The potential difference is large. It can work in dry conditions with a favourable area ratio, but in wet or marine service isolate the bolts with washers and sleeves.
Why does stainless steel appear twice?
Passive stainless steel is noble. In crevices or low-oxygen conditions it can become active, moving it much closer to carbon steel.

This calculator is a design aid. Check results against the governing code or standard and have critical work verified by a qualified engineer. Read the disclaimer.