Using the result
Keep tempering and post-weld heat treatment safely below Ac1, typically with a margin of 25 to 50 °C. For hardening, austenitise 30 to 50 °C above Ac3 so that the structure transforms fully without excessive grain growth.
Heating rate
These equations estimate temperatures for slow heating. Fast heating, as in induction hardening or welding, raises the actual transformation temperatures.
Assumptions and limits
- Slow heating rates.
- Low-alloy steels within the composition range of the original data.
References
- Andrews, K. W., Empirical formulae for the calculation of some transformation temperatures, JISI, 1965.
Questions
- What is the Ac1 of 4140?
- Roughly 730 to 750 °C depending on the analysis. Enter your heat analysis for a better estimate.
- Why does carbon appear as a square root?
- Andrews found that form best fitted the effect of carbon on Ac3 across the data set.
This calculator is a design aid. Check results against the governing code or standard and have critical work verified by a qualified engineer. Read the disclaimer.