Crack size convention
For a centre crack, a is half the total crack length; for an edge crack, a is the full depth. Geometry factors given here are for cracks small compared with the plate width; finite width, curvature and bending all change Y.
When LEFM is not enough
Tough, ductile steels yield before fast fracture. Real flaw assessments use a failure assessment diagram that combines fracture and plastic collapse, as in BS 7910 or API 579. This calculator is a first screening step.
Assumptions and limits
- Linear elastic behaviour, small-scale yielding at the crack tip.
- Mode I opening, uniform remote stress.
References
- Anderson, T. L., Fracture Mechanics: Fundamentals and Applications.
- BS 7910, Guide to methods for assessing the acceptability of flaws in metallic structures.
- API 579-1/ASME FFS-1.
Questions
- Where do I get K_IC?
- From fracture toughness tests (ASTM E399, E1820) or correlations from Charpy energy in BS 7910, which are deliberately conservative.
- Does residual stress matter?
- Yes. Welding residual stress adds to the applied stress and can be close to yield in as-welded joints.
This calculator is a design aid. Check results against the governing code or standard and have critical work verified by a qualified engineer. Read the disclaimer.